Virtual Event
- This event has passed.
Ph.D. (Engg):Thermal Sensitivity of Lamb Waves in UD-CFRP Laminates: Modeling and Experimental Validation
November 13 @ 2:00 PM - 5:00 PM
Virtual Event

Guided-wave structural health monitoring (SHM) locates damage from the arrival times of Lamb waves. Temperature, however, changes the wave velocities, and baseline subtraction then leaves false scatter that can look like real damage. In carbon-fiber-reinforced polymer (CFRP) composites the problem is more pronounced: temperature acts mainly through the matrix, so its effect depends on mode, frequency and direction. Compensation still relies on temperature-swept baselines, and the directional thermal sensitivity of unidirectional (UD) CFRP has not been characterized continuously over frequency and angle.
This thesis predicts the thermal sensitivity of Lamb waves in UD-CFRP from the measured behavior of the matrix and validates the predictions experimentally. The storage modulus of the epoxy, measured by dynamic mechanical analysis (DMA), falls by about 20 % from 30 to 70 °C. Mori-Tanaka homogenization turns this into the lamina stiffness. The fiber-dominated term C11 barely changes, while the matrix-dominated terms drop by 12-17 %. These properties feed a semi-analytical finite element (SAFE) model, which gives the velocities of the A0 and S0 modes over frequency-thickness, direction and temperature.
Directional thermal sensitivity maps of the group velocity are then built for both modes. Heating shifts the dispersion curves to lower frequency-thickness and, in general, slows both modes. The A0 sensitivity is negative and nearly uniform with frequency and direction, so a single correction can be enough. The S0 sensitivity is small at low frequency-thickness along the fibers. It grows across the fibers, where the matrix-dominated stiffness governs. Near the S0 modal transition (the veering point) it becomes large and changes sign. The maps show a closed, direction-dependent zero-sensitivity locus of S0. Along this locus the group velocity is locally insensitive to temperature. The maps also show how the locus moves as temperature rises.
For validation, a 30-ply UD-CFRP laminate was made by hand lay-up with vacuum bagging. X-ray-aligned pairs of piezoelectric wafer active sensors (PWAS) were bonded along and across the fibers for pitch-catch tests, with repeatability checks and controlled thermal cycling between 30 and 70 °C. The measurements confirm the predicted drop in group velocity in all four mode-direction configurations, and SAFE identifies the least sensitive configuration, longitudinal S0.
These results give a physics-based route from matrix DMA data to the directional thermal sensitivity of Lamb waves in UD-CFRP. They can guide temperature-resilient SHM by choosing the mode, frequency and direction that keep the thermal error low.
Keywords: Lamb waves; guided-wave SHM; CFRP laminates; thermal sensitivity; SAFE method; PWAS.